Subsurface damage in alumina and alumina-silicon carbide nanocomposites

The subsurface plastic deformation below alumina (Al 2O 3) and Al 2O 3-silicon carbide (SiC) nanocomposite surfaces subjected to grinding, polishing and annealing has been measured by high-resolution gra...

Popoln opis

Bibliografske podrobnosti
Main Authors: Tanner, B, Wu, H, Roberts, S, Hase, T
Format: Journal article
Jezik:English
Izdano: 2004