The brittle-ductile transition in single-crystal iron

The fracture behaviour of single-crystal pure iron was studied by four-point bending of pre-cracked specimens at temperatures between 77 and 180 K and strain rates between 4.46 × 10-5 and 4.46 × 10-3 s-1. Fracture behaviour changes from brittle to ductile with increasing temperature. The brittle-duc...

সম্পূর্ণ বিবরণ

গ্রন্থ-পঞ্জীর বিবরন
প্রধান লেখক: Tanaka, M, Tarleton, E, Roberts, S
বিন্যাস: Journal article
ভাষা:English
প্রকাশিত: Elsevier 2008