The production and annealing stages of the self-interstitial (R2) defect in diamond
We report on the production rate of the neutral (0 0 1)-split self-interstitial (measured via the electron paramagnetic resonance (EPR) concentration of the R2 defect) in type IIa diamond irradiated at a controlled and measured sample temperature in the interval 110-350 K with 2 MeV electrons and a...