Understanding the surface oxide evolution of T91 ferritic-martensitic steel in supercritical water through advanced characterization
The surface oxide scale formed on T91 steel after exposure to deaerated supercritical water (SCW) at 600 °C for 100-1500 h are characterized in detail to reveal the oxide evolution over time. A triplex structure with outer, inner and internal oxide layers has been confirmed. The thickness of each ox...
Hlavní autoři: | Chen, K, Shen, Z, Zhang, L |
---|---|
Médium: | Journal article |
Jazyk: | English |
Vydáno: |
Elsevier
2020
|
Podobné jednotky
-
Nanocluster evolution and mechanical properties of ion irradiated T91 ferritic-martensitic steel
Autor: Davis, TP, a další
Vydáno: (2021) -
Formation of alumina-aluminide coatings on ferritic-martensitic T91 steel
Autor: Choudhary R.K., a další
Vydáno: (2014-01-01) -
Estimation of Oxidation Kinetics and Oxide Scale Void Position of Ferritic-Martensitic Steels in Supercritical Water
Autor: Li Sun, a další
Vydáno: (2017-01-01) -
Characterization of an ASTM A335 P91 ferritic-martensitic steel after continuous cooling cycles at moderate rates
Autor: Denise Alejandra Carrizo, a další
Vydáno: (2019-01-01) -
Study on mechanical degradation of Ferrite/ martensite and austenitic steels in high-temperature supercritical carbon dioxide environment
Autor: Gen Zhang, a další
Vydáno: (2024-12-01)