THERMAL-SHOCK RESISTANCE AND BENDING STRAIN TOLERANCE OF ELECTROPHORETICALLY DEPOSITED BI2SR2CACU2OY/AG TAPES
The degradation in 77 K self-field critical current density (Jc) of electrophoretically deposited Bi-2212/Ag tapes has been evaluated separately for thermal cycling (320-77 K), bending in compression, tension and combined compression-tension. After 11 repetitions of 320-77 K thermal cycles, (Jc) is...