Fiber length, thermal, mechanical, and dynamic mechanical properties of injection-molded glass-fiber/polyamide 6,6: Plasticization effect
Unreinforced- and glass fiber-reinforced-polyamide 6,6 specimens were subjected to dry, 50 RH, and wet conditions. FLD study showed that more fiber degradation occurred during processing of the composites with higher fiber loading. TGA results revealed that about 2 and 5 levels of moisture have been...
Huvudupphovsmän: | Hassan, A., Salleh, N.M., Yahya, R., Sheikh, M.R.K. |
---|---|
Materialtyp: | Artikel |
Publicerad: |
2011
|
Ämnen: |
Liknande verk
Liknande verk
-
Tensile, impact and fiber length properties of injection-molded short and long glass fiber-reinforced polyamide 6,6 composites
av: Hassan, A., et al.
Publicerad: (2004) -
Interfacial shear strength and tensile properties of injection-molded, short- and long-glass fiber-reinforced polyamide 6,6 composites
av: Hassan, A., et al.
Publicerad: (2011) -
Moisture absorption effect on thermal, dynamic mechanical and mechanical properties of injection-molded short glass-fiber/polyamide 6,6 composites
av: Hassan, A., et al.
Publicerad: (2012) -
Sustainable basalt fiber reinforced polyamide 6,6 composites: Effects of fiber length and fiber content on mechanical performance
av: Zavier Blackman, et al.
Publicerad: (2024-07-01) -
Fibre length, thermal and mechanical properties of injection-moulded glass-fibre/polyamide 6,6 composites: effect of moisture absorption
av: Yahya, R., et al.
Publicerad: (2011)