Toughness characteristics of Arenga pinnata fibre concrete
This paper reports the results of an investigation on the toughness characteristics of concrete containing Arenga pinnata fibre. Three fibre lengths of 15 mm, 25 mm, and 35 mm were used in two volume fractions, i.e., 0.6 and 0.8. The values of toughness, first crack deflection, first crack toughness...
Main Authors: | , |
---|---|
Format: | Article |
Language: | English |
Published: |
2005
|
Subjects: | |
Online Access: | http://eprints.um.edu.my/9031/1/Toughness_Characteristics_of_Arenga_pinnata_Fibre_Concrete.pdf |
_version_ | 1796945848170446848 |
---|---|
author | Razak, H.A. Ferdiansyah, T. |
author_facet | Razak, H.A. Ferdiansyah, T. |
author_sort | Razak, H.A. |
collection | UM |
description | This paper reports the results of an investigation on the toughness characteristics of concrete containing Arenga pinnata fibre. Three fibre lengths of 15 mm, 25 mm, and 35 mm were used in two volume fractions, i.e., 0.6 and 0.8. The values of toughness, first crack deflection, first crack toughness, toughness indices, and residual strength factors are presented for ages up to 180 days. It was observed that the addition of Arenga pinnata fibre increased the toughness characteristic of concrete. However, it was observed that the positive effects of the fibre become less significant after 28 days, but still sufficient to give the concrete better toughness properties compared to the plain concrete.This is due to reaction of the fibres with the alkaline pore water in the cement matrix. © 2005 by The Haworth Press, Inc. All rights reserved. |
first_indexed | 2024-03-06T05:22:45Z |
format | Article |
id | um.eprints-9031 |
institution | Universiti Malaya |
language | English |
last_indexed | 2024-03-06T05:22:45Z |
publishDate | 2005 |
record_format | dspace |
spelling | um.eprints-90312014-10-27T05:28:25Z http://eprints.um.edu.my/9031/ Toughness characteristics of Arenga pinnata fibre concrete Razak, H.A. Ferdiansyah, T. TA Engineering (General). Civil engineering (General) This paper reports the results of an investigation on the toughness characteristics of concrete containing Arenga pinnata fibre. Three fibre lengths of 15 mm, 25 mm, and 35 mm were used in two volume fractions, i.e., 0.6 and 0.8. The values of toughness, first crack deflection, first crack toughness, toughness indices, and residual strength factors are presented for ages up to 180 days. It was observed that the addition of Arenga pinnata fibre increased the toughness characteristic of concrete. However, it was observed that the positive effects of the fibre become less significant after 28 days, but still sufficient to give the concrete better toughness properties compared to the plain concrete.This is due to reaction of the fibres with the alkaline pore water in the cement matrix. © 2005 by The Haworth Press, Inc. All rights reserved. 2005 Article PeerReviewed application/pdf en http://eprints.um.edu.my/9031/1/Toughness_Characteristics_of_Arenga_pinnata_Fibre_Concrete.pdf Razak, H.A. and Ferdiansyah, T. (2005) Toughness characteristics of Arenga pinnata fibre concrete. Journal of Natural Fibers, 2 (2). pp. 89-103. ISSN 1544-0478, DOI https://doi.org/10.1300/J395v02n02_06 <https://doi.org/10.1300/J395v02n02_06>. http://www.scopus.com/inward/record.url?eid=2-s2.0-27744538663&partnerID=40&md5=3250ed9efc31eaf59cf89b5ad4e27a66 http://www.tandfonline.com/doi/abs/10.1300/J395v02n0206#.UsucMuA5M http://www.tandfonline.com/doi/pdf/10.1300/J395v02n02₀₆ http://dx.doi.org/10.1300/J395v02n02_06 |
spellingShingle | TA Engineering (General). Civil engineering (General) Razak, H.A. Ferdiansyah, T. Toughness characteristics of Arenga pinnata fibre concrete |
title | Toughness characteristics of Arenga pinnata fibre concrete |
title_full | Toughness characteristics of Arenga pinnata fibre concrete |
title_fullStr | Toughness characteristics of Arenga pinnata fibre concrete |
title_full_unstemmed | Toughness characteristics of Arenga pinnata fibre concrete |
title_short | Toughness characteristics of Arenga pinnata fibre concrete |
title_sort | toughness characteristics of arenga pinnata fibre concrete |
topic | TA Engineering (General). Civil engineering (General) |
url | http://eprints.um.edu.my/9031/1/Toughness_Characteristics_of_Arenga_pinnata_Fibre_Concrete.pdf |
work_keys_str_mv | AT razakha toughnesscharacteristicsofarengapinnatafibreconcrete AT ferdiansyaht toughnesscharacteristicsofarengapinnatafibreconcrete |