Wire or no wire : depends on the catalyst layer thickness
Published 2013“…But with thicker layers of catalyst, no wires were found but crystalline Au particles capsulated with amorphous SiOx. …”
Get full text
Get full text
Get full text
Journal Article -
6
-
7
WIRE BREAKAGE DURING WIRE DRAWING DUE TO THE PRESENCE OF SURFACE DEFECTS, INHERITED FROM WIRE ROD
Published 2018-01-01Subjects: “…wire, wire rod, breakage, cause of breakage, surface defect, microstructure, wire drawing texture…”