Effect of Surfactant Addition on Bi2Te3 Nanostructures Synthesized by Hydrothermal Method
Published 2017-06-01“…As a result, a figure of merit of the sintered bulk sample reached 0.2 at 400 K. A maximum micro Vickers hardness of 102 Hv was obtained for the nanostructured sample, which was higher than the other reported results.…”
Get full text
Article -
1602
Analysis and characterization of 20 ppi open cell aluminum foam under mechanical loading
Published 2022-09-01“…For this purpose, three point bending test, tensile test, compression test, vickers hardness test and charpy impact test were performed to seek out the respective properties of each test. …”
Get full text
Article -
1603
Design and manufacture of computer-controlled wear device for biomedical material: A different ambient pH experimental application
Published 2023-01-01“…Composite test specimen's microhardness values were determined with Vickers hardness method before wear test procedures. …”
Get full text
Article -
1604
Effect of Hot Rolling on Microstructural Evolution and Wear Behaviors of G20CrNi<sub>2</sub>MoA Bearing Steel
Published 2021-06-01“…When the initial hot rolling reduction reached 45%, the average particle size of carbides decreased by 40%, and the area volume fraction increased by 37%. The Vickers hardness increased, but the friction coefficient and wear rate were significantly reduced with the increase in the initial hot rolling reduction. …”
Get full text
Article -
1605
-
1606
Research on Roughness and Microhardness of C45 Material Using High-Speed Machining
Published 2023-07-01“…The main purpose of the article is to create a comprehensive overview of the behavior and properties of the selected material with a focus on the prediction of roughness depending on the cutting speed and depth of cut, Vickers microhardness evaluation, assessment of cutting tool wear, and assessment of the shape and structure of the resulting chip. …”
Get full text
Article -
1607
Effect of increasing the Al2O3 content on the phase formation and mechanical properties of lithium disilicate glass-ceramics
Published 2021-01-01“…For the lowest content of Al _2 O _3 , the highest flexural strength and Vickers hardness were obtained as 188.34 MPa and 776 HV, respectively. …”
Get full text
Article -
1608
Microstructure evolution and mechanical properties of hot deformed Mg9Al1Zn samples containing a friction stir processed zone
Published 2017-12-01“…Samples deformed at 350 °C revealed an increment of ductility that was doubled as compared to those deformed at 300 °C and a strengthening of the nugget was measured by Vickers microhardness (HV). The correlation of HV average values to local grain size confirmed the validity of the Hall–Petch type equation where stress is replaced by hardness. …”
Get full text
Article -
1609
Structural Stability of the SUPER304H Steel Used in Energetics
Published 2022-01-01“…Mechanical properties were evaluated by Vickers hardness and tensile tests. The microstructure was observed using light optical microscopy (LOM) and scanning electron microscopy (SEM) with the energy-dispersive X-ray detector (EDXS). …”
Get full text
Article -
1610
Interface Control in Additive Manufacturing of Dissimilar Metals Forming Intermetallic Compounds—Fe-Ti as a Model System
Published 2020-10-01“…Electron backscatter diffraction (EBSD) was performed in addition to EDS to identify the crystalline phases. The Vickers hardness test was conducted in areas with different phases. …”
Get full text
Article -
1611
Low-Roughness-Surface Additive Manufacturing of Metal-Wire Feeding with Small Power
Published 2021-07-01“…The ultimate tensile strength of the specimens measured about 500 MPa, the relative density was 99.37, and the Vickers hardness was homogeneous. The results show that the proposed laser-Joule wire feed-direct metal deposition process (LJWF-DMD) is a very attractive solution for metal AM of high surface quality parts, particularly suitable for rapid prototyping for on-orbit AM in space.…”
Get full text
Article -
1612
Effect of grain growth in bimodal microstructure on cutting performance of self-toughening Dy-α-SiAlON ceramic tool inserts
Published 2023-09-01“…The results showed good Vickers hardness (19.0-19.7GPa) and fracture toughness (3.61-4.18MPa•m1/2) increasing with crack propagation length. …”
Get full text
Article -
1613
Study of root canal isthmus dentin structure and mineral content and microhardness
Published 2020-10-01“…Methods Thirty single-root premolars with a canal isthmus (experimental group) and thirty single-root premolars without a canal isthmus (control group) were collected and analyzed by scanning electron microscopy, X-ray energy spectrometry and a Vickers microhardness tester. Structure, mineral content and microhardness were compared. …”
Get full text
Article -
1614
Deposition of Nickel-Based Superalloy Claddings on Low Alloy Structural Steel by Direct Laser Deposition
Published 2021-08-01“…Scanning electron microscopy, energy dispersive spectroscopy, and electron backscatter diffraction were performed for microstructural characterisation. The Vickers hardness test was used to analyse the mechanical response of the optimised cladding layers. …”
Get full text
Article -
1615
Characteristics of Natural Fiber Composites Materials Reinforced with Aluminum and Copper Powder for The Performance of Automatic Motorcycle Clutch Pad
Published 2023-08-01“…Hardness testing using the Vickers method and testing the performance of automatic motorbikes with a chassis dyno test. …”
Get full text
Article -
1616
PHYSICAL AND MECHANICAL PROPERTIES OF HYDROXYAPATITE CERAMICS WITH A MIXTURE OF MICRON AND NANO-SIZED POWDERS: OPTIMISING THE SINTERING TEMPERATURES
Published 2021-09-01“…The mechanical properties are maintained at a high level at sintering temperatures of 1150 °C and 1200 °C, i.e., Vickers hardness values of 4.40 GPa and 5.67 GPa, respectively.…”
Get full text
Article -
1617
Mechanical Properties of Explosion-Welded Titanium/Duplex Stainless Steel under Different Energetic Conditions
Published 2022-08-01“…The differences between the two welding conditions were compared using a tensile test, fracture analysis, a 90° bending test, Vickers hardness, and nanoindentation related to the mechanical properties of materials. …”
Get full text
Article -
1618
Correlations between the Surface Topography and Mechanical Properties of Friction Stir Welds
Published 2020-07-01“…This study explored the connections between the surface topography of the welds, such as the flash height and the seam underfill, and their mechanical properties (ultimate tensile strength; elongation at break; and Vickers hardness). For this purpose, a total of 54 welding experiments at three different welding speeds were conducted using the aluminum alloy EN AW-6082-T6. …”
Get full text
Article -
1619
Evaluation of flexural strength, degree of conversion, and demineralization-prevention properties in adjacent tooth structures of an experimental fissure sealant containing nano-ca...
Published 2023-11-01“…To evaluate the demineralization-prevention ability, Cl V cavities in 10 third molar teeth restored with two sealant products, followed by an acid challenge then the Vickers microhardness test was carried out. Results The mean flexural strength in the commercial group was higher than the experimental group. …”
Get full text
Article -
1620
Mechanical Properties and Corrosion Behavior of Thermally Treated Ti-6Al-7Nb Dental Alloy
Published 2022-05-01“…The microstructure was investigated, and the mechanical characterization was carried out by Vickers microhardness test. Young’s modulus measurements and tensile tests were performed in order to study the effect of cooling media on the material. …”