1641
Sintering studies of synthesised manganese-oxide-doped calcium phosphate via wet chemical precipitation method
Published 2014“…The results also revealed that 0.3 wt% MnO2-doped biphasic calcium phosphate gave a maximum Vickers hardness of 5.14 GPa. On the other hand, 1.0 wt% MnO2-doped biphasic calcium phosphate exhibited highest fracture toughness of 1.32 MPa m(1/2) as compared to 0.88 MPa m(1/2) for undoped biphasic calcium phosphate when sintered at 1200 degrees C.…”
Article -
1642
Effect of Dental Restorative Material Type and Shade on Characteristics of Two-Layer Dental Composite Systems
Published 2016“…Micro-indentation experiment was performed on the bulk and also on each layer of layered restoration specimens using a Vicker’s indenter. The interface between the two layers was studied by scanning electron microscopy (SEM). …”
Get full text
Article -
1643
Sintering behavior of anorthite-based composite ceramics produced from natural phosphate and kaolin
Published 2019“…The composite ceramics were sintered in air at various temperatures ranging from 1250 °C to 1325 °C and characterized to determine the phase present, relative density, Vickers microhardness, chemical bonding of molecules and microstructural development. …”
Article -
1644
Densification behaviour and properties of manganese oxide doped Y-TZP ceramics
Published 2011“…Bulk density, Young's modulus, Vickers hardness and fracture toughness tests were carried out on the sintered samples. …”
Article -
1645
Fabrication of functionally graded Hydroxyapatite-Titanium by applying optimal sintering procedure and powder metallurgy
Published 2011“…Result from optical micrograph and SEM indicate that the HA/Ti FG cylinder can be produced successfully by cold pressing with developed thermal mapping. Vicker’s hardness of HA/Ti is higher than that of pure microcrystalline Ti (metal) and reduces by decreasing the density of the layer of HA/Ti.…”
Get full text
Article -
1646
Carbosilisiothermic reduction of rutile to produce nano-sized particles of TiC and its composite with SiO2
Published 2014“…The fracture toughness, and Vickers hardness values of the TiC-SiO2 nanocomposite are measured to be 3.82 MPa m1/2 and 19.9 GPa, respectively. …”
Get full text
Article -
1647
Mechanical properties of titanium-hydroxyapatite (Ti-HA) composite coating on stainless steel prepared by thermal spraying
Published 2017“…The hardness and strength was determined by using SHIMADZU-microhardness Vickers tester and PosiTest AT portable adhesion tester respectively. …”
Get full text
Conference or Workshop Item -
1648
Wear And Friction On Gimbal Sealant
Published 2018“…The testing process were done by measuring the wear and friction using the pin-on-disc machine (POD), profilometer machine, Vickers hardness testing machine, and universal testing machine (UTM). …”
Get full text
Monograph -
1649
Structural Integrity Investigation Of SAC305 Lead Free Solder
Published 2022“…The effect of IMCs in the terms of hardness was investigated using Vickers hardness test and nanoindentation. A specific indentation array was performed on four different horizontal cross sections of the solder with different heights and diameters. …”
Get full text
Monograph -
1650
The influence of welding condition on the microstructure of WC hardfacing coating on carbon steel substrate
Published 2019“…The effects of the welding parameters on WC hardfacing coating microstructure and hardness value were characterized by scanning electron microscope (SEM) and micro-Vickers hardness tester respectively. The larger carbide growth in overall coating region is mainly dictated by high current (200 A), increased number of weld layers (3 layers) and presence of base material preheat due to sufficient heat energy initiating carbide growth. …”
Get full text
Article -
1651
Physical and structural properties of Nd : YAG crystal growth by czocharalski method
Published 2012“…It was also discovered that Vickers hardness increased with increasing dopant concentration which was from 1590 Hv to 1776 Hv. …”
Get full text
Thesis -
1652
Mechanical properties of stabilized zirconia nanocrystalline eb-pvd coating evaluated by micro and nano indentation
Published 2013“…substrate preheating temperature produced the highest hardness value of about 21.7 GPa. Vickers micro hardness was utilized with the aid of the Tabor equation in order to achieve deeper insight into the correlation between adhesion and deposition process parameters.…”
Article -
1653
Effect of pretreatment process on thermal oxidation of biomedical grade cobalt based alloy
Published 2012“…The metallic compositions, surface morphology and hardness of the oxide layer formed on the substrate were verified using X-ray diffraction (XRD), scanning electron microscope and micro-Vickers hardness analysis respectively. It is found that mechanical pretreatment provides oxide/carbide layer with higher hardness than chemical pretreatment method. …”
Article -
1654
A novel hydroxyapatite composite reinforced with titanium nanotubes coated on Co-Cr-based alloy
Published 2015“…In addition, the mechanical properties of the composite layer including Vickers micro-hardness and bonding strength were examined. …”
Article -
1655
Strengthening of the mechanical and tribological properties of composite oxide film formed on aluminum alloy with the addition of graphite
Published 2020“…The microhardness was characterized at the surface and cross-section of the films by Vickers microhardness tester. The structure of the oxide films and graphite were studied by X-ray diffractometer (XRD) and Raman spectroscopy. …”
Article -
1656
Microstructural characterization, mechanical and tribological properties of ZC71 hybrid composite reinforced with SiC and MWCNT
Published 2021“…The results revealed that the proper amount/size of SiC particles with the addition of MWCNTs had a considerable effect on the microstructural alteration, and mechanical and tribological properties of the ZC71 alloy. The Vickers hardness values of the ZC71 alloy improved with the addition of MWCNT and SiC. …”
Get full text
Article -
1657
Mechanical and Microstructural Characterization of AA6061- AA7075 Dissimilar Friction Stir Welding
Published 2015“…Mechanical property analysis of specimens was conducted using tensile test and Vickers hardness test. Meanwhile, microstructure characterization of the optimum sample was conducted using optical microscope, scanning electron microscopy (SEM) and energy dispersive X-ray spectroscopy (EDS). …”
Get full text
Get full text
Conference or Workshop Item -
1658
Fabrication & properties of aluminium-silicon carbide (A1/SiC) composite material
Published 2015“…After that, the hardness of composites was tested by using Vickers Micro-Hardness Testing machine. The conclusion gained from this study is the different ceramic composition under various compaction loads plays significant influences in determining the performances of the Al/SiC composite material. …”
Get full text
Undergraduates Project Papers -
1659
Effect of weight percentage of silicon carbide (SiC) reinforcement particles on mechanical behavior of aluminum metal matrix composite (Al MMC)
Published 2008“…The effect of weight percentage of silicon carbide on hardness of composites was investigated by using Vickers hardness Test. It was observed that the distribution of silicon carbide particles was uniform. …”
Get full text
Undergraduates Project Papers -
1660
Deposition of Electroless Nickel Boron as Printed Circuit Board Surface Finish
Published 2016“…For mechanical properties, the hardness test was conducted by using Vickers Hardness Test MMT-X7 Matsuzawa and surface structure was evaluate using ProgRes C3 IM7200 Optical Microscope and Field Emission Scanning Electron Microscopy (FESEM). …”
Get full text
Article