1841
Evaluation of the Wear and Mechanical Properties of Titanium Diboride-Reinforced Titanium Matrix Composites Prepared by Spark Plasma Sintering
Published 2023-03-01“…This indicates that the SPS process aids good sinterability. The Vickers hardness of the consolidated samples improved from 188.1 HV1 to 304.8 HV1, attributed to the high hardness of the TiB<sub>2</sub>. …”
Get full text
Article -
1842
Indentation, finite element modeling and artificial neural network studies on mechanical behavior of GFRP composites in an acidic environment
Published 2023-05-01“…In this study, the indentation tests are performed with various forces using the Vickers indenter to investigate the mechanical properties, including the elastic modulus, hardness, and the plasticity index of pure, and incorporated glass fiber reinforced polymer (GFRP) composites with nanosilica and nanoclay. …”
Get full text
Article -
1843
Effect of enzymatic degradation and hydrolysis on 3D-printed resin-based composite material for temporary dental crowns and bridges
Published 2022-09-01“…Surface roughness of polished specimens was measured by AFM and hardness with a Vickers micro hardness tester. After enzymatic degradation and hydrolysis, BisGMA was detected in the eluates of the additively manufactured composites. …”
Get full text
Article -
1844
The effect of different curing distances on the microhardness of flowable bulk-fill composite materials
Published 2023-12-01“…Microhardness was measured using the Vickers test with a 50-g load for 15 seconds for the top and bottom surfaces of all the samples. …”
Get full text
Article -
1845
Fabrication of SiCw/Ti3SiC2 composites with improved thermal conductivity and mechanical properties using spark plasma sintering
Published 2020-07-01“…The bending strength of 10 wt% SiCw/Ti3SiC2 was 635 MPa, which was approximately 50% higher than that of the monolithic Ti3SiC2 (428 MPa). The Vickers hardness and thermal conductivity (k) also increased by 36% and 25%, respectively, from the monolithic Ti3SiC2 by the incorporation of 10 wt% SiCw. …”
Get full text
Article -
1846
High cycle fatigue and corrosion behaviors of Mg3Zn/HA biodegradable composite
Published 2024-01-01“…The results of the microstructural evaluation showed that grain refinement occurred in the composite by 48 % and Vickers microhardness increased approximately by 12 %. …”
Get full text
Article -
1847
Impacts of Lubricant Type on the Densification Behavior and Final Powder Compact Properties of Cu–Fe Alloy under Different Compaction Pressures
Published 2022-08-01“…The systematic evolution of the densification, porosity, and pore-size behavior were studied. Vickers Hardness Tests were used to measure hardness. …”
Get full text
Article -
1848
In-situ synthesis and chemical bonding of the Al-doped β-SiC particles in Al-Si-C light alloys
Published 2022-12-01“…It is also found that the Young’s modulus and Vickers hardness of doped SiCp decrease as the Al doping content increases by DFT calculations. …”
Get full text
Article -
1849
Effect of Artificial Saliva Modification on the Corrosion Resistance and Electronic Properties of Bego Wirobond<sup>®</sup> C Dental Alloys
Published 2023-11-01“…The CoCrMo alloy was characterized by a Vickers microhardness value of 445(31) µHV<sub>0.3</sub>. …”
Get full text
Article -
1850
Joining of Zirconia to Ti6Al4V Using Ag-Cu Sputter-Coated Ti Brazing Filler
Published 2022-02-01“…Room temperature shear tests and Vickers microhardness tests performed across the interfaces were used to evaluate the mechanical strength of the joints. …”
Get full text
Article -
1851
An investigation on microstructure and mechanical behaviour of copper-nickel coated carbon fibre reinforced aluminium composites
Published 2020-01-01“…When compared with as-cast alloy and Ni coated CF reinforced composite, the tensile strength of Cu coated CFs composite was higher by 15.36% and 2.55%. Similarly, micro-Vickers hardness was improved by 7.61% and 3.09%, impact strength by 19.61% and 3.39%, flexural strength by 87.50% and 15.38%. …”
Get full text
Article -
1852
Investigation of Corrosion Behavior for Copper-Based Shape Memory Alloys in different Media
Published 2017-06-01“…After samples preparation examination were done by using XRD, SEM technique, DSC, Vickers hardness, Archimedes method to measure the porosity percentage and corrosion rate in different solutions (HCl, NaOH and SEAWATER).The XRD and microstructure results show that all samples with and without additives consist of two phases (β-phase) and (α-phase) at room temperature and the addition of alloying elements in these percentages does not have effect on present phases. the hardness increased with zinc content because the formation of intermetallic compound of CuZn that responsible to hardness while The addition of Si ,Sn and Ni leads to lower the hardness than aluminum. …”
Get full text
Article -
1853
The Contribution of Local Muslim Scholars to the Development of Indonesia’s Education
Published 2022-12-01“…Since Islam was first introduced in Indonesia, its spreading has been inseparable from people’s daily lives, including the building and shaping of the education sector (Rochmawati et al., 2018; Vickers, 2013; Hasan, 2009). Java Island is one of Indonesia’s regions with a wider history of Islamic education (Ricklefs, 2012; Woodward, 2010). …”
Get full text
Article -
1854
First-Principles Study on III-Nitride Polymorphs: AlN/GaN/InN in the <i>Pmn</i>2<sub>1</sub> Phase
Published 2020-07-01“…The mechanical properties reveal that <i>Pmn</i>2<sub>1</sub>-AlN and <i>Pmn</i>2<sub>1</sub>-GaN possess a high Vickers hardness of 16.3 GPa and 12.8 GPa. <i>Pmn</i>2<sub>1</sub>-AlN, <i>Pmn</i>2<sub>1</sub>-GaN and <i>Pmn</i>2<sub>1</sub>-InN are all direct semiconductor materials within the HSE06 hybrid functional, and their calculated energy band gaps are 5.17 eV, 2.77 eV and 0.47 eV, respectively. …”
Get full text
Article -
1855
Adhesiveness of TiO2 PVD coating on electropolished stainless steel 17–4 PH orthodontic bracket
Published 2019-01-01“…The coating quality on the substrates with different roughness was assessed through coating adhesivity on the substrate by micro Vickers qualitatively. The results showed that the TiO _2 coating layer on the substrate with a lower roughness had better adhesivity rather than on the substrate with higher roughness.…”
Get full text
Article -
1856
PENGECORAN ALUMINIUM MATRIKS KOMPOSIT BERPENGUAT CARBON NANOTUBE (CNT) DENGAN VARIASI PENAMBAHAN SERBUK MAGNESIUM
Published 2023-12-01“…The samples were then analyzed for mechanical properties and microstructure observations. The results of the Vickers hardness test before the addition of Mg powder and CNT were 36.7 HV. …”
Get full text
Article -
1857
Characterization and Modification of Red Mud and Ferrosilicomanganese Fines and Their Application in the Synthesis of Hybrid Hydrogels
Published 2022-10-01“…Regarding the synthesis of the hybrid hydrogels, it was determined that the incorporation of small percentages (0.1%) of the inorganic phases improved the capacity of the materials to absorb water (swelling indices of 1678% and 1597% for the RM and FeSiMn hydrogels, respectively) compared to the conventional polyacrylamide hydrogel (1119%). An improvement in Vickers microhardness and storage modulus (G′) was also observed: the hybrid with 10% RM presented a G′, 50 times higher than conventional hydrogel. …”
Get full text
Article -
1858
Effect of Two-liquid Bimetal Wear Resistance Plate Thickness on Microstructures and Properties of Composition Layer
Published 2016-08-01“…The results show that, the sequence of the microstructure from the low carbon steel to the high chromium cast iron is as follows:low carbon steel→pearlite transition layer→composition layer→high chromium cast iron transition layer. The Vickers hardness of composition layer region is from 345 to 1260. …”
Get full text
Article -
1859
Effect of growth conditions on the mechanical properties of lanthanum-gallium tantalate crystals
Published 2020-07-01“…The microhardness HV of the specimens was measured with an DM 8B Affri microhardness tester by Vickers methods. The hardness H, elastic modulus E and elastic recovery coefficient R were measured with a Berkovich pyramid on a CSM Nano-Hardness Tester using the instrumented indentation (nanoindentation) method. …”
Get full text
Article -
1860
Effect of Thermal History on Microstructures and Mechanical Properties of AZ31 Magnesium Alloy Prepared by Friction Stir Processing
Published 2014-02-01“…Transmission electron microscopy (TEM) examinations confirm that grain refinement is attributed to continuous dynamic recrystallization both for NFSP and SFSP. The average Vickers hardness in the SZ of the NFSP and SFSP AZ31 magnesium alloy are 76 HV and 87 HV. …”