    Linerboard made from Soda-Anthraquinone (Soda-AQ) treated coconut coir fiber and effect of pulp beating by Main, Nor Mazlana, A. Talib, Rosnita, Ibrahim, Rushdan, Abdul Rahman, Russly, Mohamed, Ainun Zuriyati

    Published 2015
    “…Out of nine pulping conditions characterized, a pulping condition of 18% active alkali for 90 min cooking time was chosen. These conditions provided the highest screened yield (48.99%), a low rejection yield (0.27%), high viscosity (11.73 cP), and a kappa number (41) that is acceptable for unbleached linerboard production. …”