Showing 3,161 - 3,180 results of 5,428 for search '((min OR (spie OR penggged)) OR (((long OR lin) OR ssspinga) OR link))', query time: 0.15s Refine Results
  1. 3161
  2. 3162
  3. 3163
  4. 3164
  5. 3165

    Surface modification of additive manufactured components by ultrasonic cavitation abrasive finishing by Tan, Kai Liang, Yeo, Song Huat

    Published 2017
    “…Results have demonstrated that this technique improves Ra values of as-built Inconel 625 side surfaces by up to 45% after 30 min of processing time. Scanning electron microscopic images revealed that most small-sized partially melted powders were removed through heterogeneous cavitation nucleation on the specimens’ rough initial surface. …”
    Get full text
    Get full text
    Journal Article
  6. 3166
  7. 3167
  8. 3168
  9. 3169
  10. 3170
  11. 3171
  12. 3172
  13. 3173
  14. 3174
  15. 3175
  16. 3176

    Temperature and stress distribution in the SOI structure during fabrication by Tan, Cher Ming, Gan, Zhenghao, Gao, Xiaofang

    Published 2009
    “…Although it is expected that the furnace temperature and withdrawal velocity are the key factors in determining the mechanical stresses, for the present bonding strength of wafers via wafer bonding technology, the withdrawal velocity must be less than 100 mm/min, and under such a withdrawal velocity, the furnace temperature is also an insignificant factor with regard to the induced stress.…”
    Get full text
    Get full text
    Journal Article
  17. 3177

    Effect of processing parameters on electroless Cu seed layer properties by Chen, Z., Chan, L., See, Alex K. H., Law, S. B., Zeng, K. Y., Shen, L., Tee, K. C., Ee, Elden Yong Chiang

    Published 2012
    “…Of particular interest is that there exists a preferred Cu (111) crystal orientation in the samples subjected to more than as short as 3 min of deposition. A surface roughness (Rrms) of ∼17 nm has been achieved. …”
    Get full text
    Get full text
    Journal Article
  18. 3178
  19. 3179

    Spark plasma reaction sintering of ZrO2-mullite composites from plasma spheroidized zircon/alumina powders by Yu, L. G., Li, Y., Munir, Z. A., Khor, Khiam Aik, Dong, Zhili

    Published 2012
    “…Mullite-zirconia ceramic composites are prepared by reaction sintering of plasma spheroidized (PS) zircon-alumina powders in a spark plasma sintering (SPS) system at 1000, 1100, 1200 and 1300 °C with duration of 10 and 30 min. At SPS temperature of 1000 °C, evidence of zircon decomposition is detected, while at 1200 °C, mullite formation dominates the process, resulting in significant increases in microhardness, Young’s modulus and fracture toughness values. …”
    Get full text
    Get full text
    Journal Article
  20. 3180

    The Brazilian disc test for rock mechanics applications : review and new insights by Li, Diyuan, Wong, Louis Ngai Yuen

    Published 2013
    “…A simple extension strain criterion was put forward by Stacey (Int J Rock Mech Min Sci Geomech Abstr 18(6):469–474, 1981) to account for extension crack initiation and propagation in rocks, although this is not widely used. …”
    Get full text
    Get full text
    Journal Article