    Densification behaviour and sintering mechanisms of Cu- or Co-doped SnO2 : a comparative study by Zhang, T. S., Kong, Ling Bing, Song, X. C., Du, Z. H., Xu, W. Q., Li, S.

    Published 2014
    “….% Cu- or Co-doped SnO2 ceramics could reach over 95% relative density when sintered to 1250 °C with a heating rate of 5 °C min−1. It was found that both CoO4/3- and CuO-doped SnO2 follow the same mass transport mechanism – viscous flow sintering during early-stage sintering. …”
    Get full text
    Get full text
    Journal Article
  16. 816

    Microbiological, physicochemical and nutritional properties of fresh cow milk treated with industrial high pressure processing (HPP) during storage by Lim, Shu Huey, Chin, Nyuk Ling, Sulaiman, Alifdalino, Tay, Cheow Hwang, Wong, Tak Hiong

    Published 2023
    “…The safety, shelf life, and quality of fresh cow milk treated using industrial High-Pressure Processing (HPP) treatment at 600 MPa for 10 min was studied to identify the novelty of this non-thermal technology in milk processing. …”
    Get full text
    Article
  17. 817
  18. 818
  19. 819
  20. 820