Hydroxyapatite coating with oxide interlayer on biomedical grade cobalt based alloy

Surface modification is often required in order to improve the biological and tribological properties of metallic implants. In this research, Co-Cr-Mo alloy was oxidized in atmospheric condition to create oxide interlayer (Cr2O3) at different temperatures (850°C, 1050°C and 1250°C) for 3 hours prior...