Effect of Cobalt Doping and Milling Time on Microstructure and Vickers Microhardness of the Spark Plasma Sintered (67-x)Ti-xCo-22Si-11B (x = 2 and 6 at-%) Alloys
Abstract Ti-6Al-4V and TiAl-based alloys are widely used for fabricating the implantable orthopedic devices and automotive components, respectively. Ti6Si2B-based alloys are attractive for use in orthopedic components because their higher hardness, superior biocompatibility and corrosion resistance...