Microstructure and transformation characteristics of a TiAlNb alloy with Cr and Mo addition

The present study investigated the Ti-46Al-4Nb-2Mo and Ti-46Al-4Nb-2Cr (at.%) alloys, which were prepared by solution treatment at 1,400 °C for 30 minutes prior to being air-cooled. The alloys were subsequently reheated to 1350 °C for 60 minutes and were cooled to room temperature by oil or water qu...