Corrosion-Erosion Waste of Metals in the Duct System of the Recycling Aluminium Furnace
The corrosion aggressiveness of the environment in the recycling aluminium furnace duct system is very high. Temperature is in the range from 300 to 900 °C and chemical composition of combustion varies according to treated aluminium waste and flue gas flow is turbulent. These conditions are very com...