Mechanical and Microstructural Response of Near Beta Ti Alloys to Hot Tensile Testing

Hot tensile tests were carried out on Timetal-125 and Timetal-LCB near beta Ti alloys at temperatures in range of 600-1000°C and constant strain rate of 0.1 s−1. At temperatures below 700-800°C, the homogenuous and total strains for Timetal-LCB were greater than those for Timetal-125. In contrast, a...