Microstructure and fractal characteristics of the solid-liquid interface forming during directional solidification of Inconel 718
The solidification microstructure and fractal characteristics of the solid-liquid interfaces of Inconel 718, under different cooling rates during directional solidification, were investigated by using SEM. Results showed that 5 μm/s was the cellular-dendrite transient rate. The prime dendrite arm sp...