Mechanical behaviour of porous metals fabricated by low-power selective laser melting

In selective laser melting (SLM) metal powder is completely melted using a high-power laser beam of 200-400 W to form metallic parts which are almost completely dense and do not require post processing. To reduce the effective Young's modulus of fabricated parts by SLM to that of human bone...