In- and out-of-phase thermomechanical fatigue of a Ni-based single-crystal superalloy
In this study, the difference between in-phase (IP) and out-of-phase (OP) thermomechanical fatigue (TMF) cycling from 100 to 750 °C has been investigated for the Ni-based single-crystal superalloy MD2. In addition, two different crystal orientations were studied, the ⟨001⟩ and ⟨011⟩ orientations res...