Improving strength and ductility of Ti-4Al-0.005B titanium alloy through tailoring equiaxed and lamellar microstructure during thermal mechanical process

The Ti-4Al-0.005B alloy were rolled at 940 °C or 990 °C followed by annealing at 650 °C. In order to control the final microstructure, rolling at medium temperature of 550 °C was processed in two other plates after rolling at 940 °C or 990 °C. The rolling and tensile behaviors of Ti-4Al-0.005B alloy...