Two plates of thixoformed 7075 aluminum alloy were joined using Electron Beam Welding (EBW). A post-welding-heat treatment (PWHT) was performed within the semi-solid temperature range of this alloy at three temperatures, 610, 617 and 628 °C, for 3 min. The microstructural evolution and mechanical pr...