Criteria of Activation of Powdery Materials by a Preliminary Mechanical Treatment
γ-Fe2O3 was vibration ball-milled with varying amplitude, α, from 8 to 24mm and grinding time. The enthalpy increase, ΔH*, due to mechanical treatment was measured by a differential scanning calorimeter. Pretreated sample was subsequently heated at 693K for 60min, and the fractional transformation i...
Main Author: | Mamoru Senna |
---|---|
Format: | Article |
Language: | English |
Published: |
Hosokawa Powder Technology Foundation
2014-06-01
|
Series: | KONA Powder and Particle Journal |
Online Access: | https://www.jstage.jst.go.jp/article/kona/1/0/1_1983009/_pdf/-char/en |
Similar Items
-
The Evaluation of Activity and Reactivity of Mechanically Treated Fine Powdered Materials
by: Mamoru Senna
Published: (2014-06-01) -
Pore Size Distribution of Cast, Compressed and Lightly Sintered Alumina with Preliminary Mechanical Treatments
by: Katsuhiro Kobayashi, et al.
Published: (2014-05-01) -
The Optimization of Mechanochemical Processes toward Functional Nanocomposite Materials
by: Mamoru Senna
Published: (2023-09-01) -
Mechanisms of resistance to powdery mildew in cucumber
by: Mumin Ibrahim TEK, et al.
Published: (2022-05-01) -
OPTICAL PROPERTIES OF FIBROUS AND POWDERY MATERIALS WITH NANOSTRUCTURED CONDUCTIVE COATINGS
by: V. A. Bogush
Published: (2019-06-01)