Quasi-Static Fracture Toughness and Damage Monitoring in Liquid Metal Reinforced Hybrid Composites
An experimental study is performed to investigate the quasi-static fracture toughness and damage monitoring capabilities of liquid metal (75.5% Gallium/24.5% Indium) reinforced intraply glass/carbon hybrid composites. Two different layups (G-0, where glass fibers are along the crack propagation dire...