Investigation of zinc stannate synthesis using photoacoustic spectroscopy

Mixtures of ZnO and SnO2 powders, with molar ratio of 2:1, were mechanically activated for 40, 80 and 160 minutes in a planetary ball mill. The resulting powders were compacted into pellets and non-isothermally sintered up to 1200°C with a heating rate of 5°C/min. X-ray diffraction analysis of obtai...

Full description

Bibliographic Details
Main Authors: Ivetić T., Nikolić M.V., Nikolić P.M., Blagojević V., Đurić S., Srećković T., Ristić M.M.
Format: Article
Language:English
Published: International Institute for the Science of Sintering, Beograd 2007-01-01
Series:Science of Sintering
Subjects:
Online Access:http://www.doiserbia.nb.rs/img/doi/0350-820X/2007/0350-820X0702153I.pdf