Corrosion of N10276 in a H<sub>2</sub>S, HCl, and CO<sub>2</sub> Containing Atmosphere at 480 °C and 680 °C
In several industrial processes, metallic materials suffer from chlorine- and sulfur-induced high-temperature corrosion. In previous studies, several steels have been tested at laboratory scale in a simulated gas atmosphere of a pyrolysis process of anthropogenic resources. In this paper, we propose...