Compressive Deformation Behavior of an Ultrafine/Nano Grained AZ31 Magnesium Processed by Accumulative Back Extrusion

An AZ31magneium alloy was processed through accumulative back extrusion (ABE) process at 280 °C up to six passes. Compressive deformation behavior of the processed materials was studied by employing uniaxial compression tests at room temperature. The results indicated that grains of 80 nm to 1 µm si...