Investigation of the effect of pressure, sintering temperature and time on silicon carbide microstructure

In this research, SiC ceramics were densified via spark plasma sintering (SPS) with 0.5wt.% B4C and 1.5wt.% C additions at temperatures ranging from 1900 to 2000°C for 5-65min under 10-50MPa applied pressure with an intermediate dwell at 1400°C, and the effects of applied pressure, sintering tempera...