Deterioration mechanism of Al2O3–MgO refractory castable in RH refining ladle

The purpose of this work was to investigate the deterioration mechanism of an optimized Al2O3–MgO refractory castable during industrial trials. After structural optimization, the average corrosion rate of every cycle deceased to 0.29 mm/cycle from 0.46 mm/cycle. Corroded microstructure of the optimi...

Full description

Bibliographic Details
Main Authors: Junfeng Chen, Yu Zhang, Guangping Liu, Guoping Wei, Yi Zhao, Wen Yan, Nan Li
Format: Article
Language:English
Published: Elsevier 2023-12-01