X-ray data about the structural response of melt-spun poly(3-hydroxybutyrate) fibers to stress and temperature

Mechanical properties of as-spun, aged and stress-annealed melt-spun poly(3-hydroxybutyrate) (P3HB) fibers are presented in section 1.1. Section 1.2 presents tables with stress/temperature conditions and exposure times during in-situ laboratory WAXD and SAXS experiments, and section 1.3 presents azi...