Influence of thermomechanical processing on coarse particles, grain structure, and mechanical properties of Al–Cu alloy rings

Rings made of 2219 Al alloy are typically manufactured by multi-directional forging (MDF) and ring rolling at 460 °C, followed by heat treatment. However, this process often results in coarse elongated grains and a large number of coarse Al2Cu particles, resulting in rings with poor mechanical prope...