Synthesis of barium-zinc-titanate ceramics

Mixtures of BaCO3, ZnO and TiO2 powders, with molar ratio of 1:2:4, were mechanically activated for 20, 40 and minutes in a planetary ball mill. The resulting powders were compacted into pellets and isothermally sintered at 1250°C for 2h with a heating rate of 10°C/min. X-ray diffraction analysis...