Effects of Zn content on Hot Tearing Susceptibility of Mg–7Gd–5Y–0.5Zr Alloy
Mg−7Gd−5Y−0.5Zr alloy has excellent mechanical properties but poor hot tearing resistance. The latter makes it difficult to cast billets, which limits the size of subsequently processed parts. Therefore, the hot tearing susceptibility of Mg−7Gd−5Y&am...