The Hot Tensile Properties, Fracture Features, and Microstructure Evolution of As-Cast 7005 Aluminum Alloy
In order to explore the hot deformation behaviors of the as-cast 7005 aluminum alloy, a number of hot tensile tests with four temperatures (100, 200, 300, and 400 °C) and three strain rates (0.001, 0.01, and 0.1 s<sup>−1</sup>) were performed. The Johnson–Cook model was used to express t...