Roughness of the nuclear reactor pipe inner surface depending on the reactor operating time

During operation of nuclear reactors, there are various factors that affect the nuclear plant piping leading to erosion of the pipe inner surface and an increase of its micro-relief (roughness). Metal corrosion occurs and spreads faster on a surface having a higher value of the roughness parameter....

Full description

Bibliographic Details
Main Authors: Maksim A. Trofimov, Ruslan A. Globa
Format: Article
Language:English
Published: National Research Nuclear University (MEPhI) 2019-12-01
Series:Nuclear Energy and Technology
Subjects:
Online Access:https://nucet.pensoft.net/article/48394/download/pdf/