Effect of trialkoxysilane/aminosilane-containing universal adhesive on resin-ceramic microtensile bond strength and ceramic wettability: An in-vitro study
Background: The dual-silane (trialkoxysilane/aminosilane) universal adhesive (UA) is claimed for its enhanced priming capacity of glass-ceramics. Objective: This study evaluated the effect of organofunctional trialkoxysilane- and organofunctional trialkoxysilane/aminosilane-containing UAs on the lon...