Role of CdTe Interface Structure on CdS/CdTe Photovoltaic Device Performance
Glancing angle deposition (GLAD) of CdTe can produce a cubic, hexagonal, or mixed phase crystal structure depending upon the oblique deposition angles (Φ) and substrate temperature. GLAD CdTe films are prepared at different Φ at room temperature (RT) and a high temperature (HT) of 250 °C and used as...