Development of an ω-Phase in Grade 2 Titanium Processed by HPT at High Hydrostatic Pressure

High-pressure torsion was used to process grade 2 titanium to 10 turns using different pressures up to a maximum of 8 GPa. X ray diffraction showed that the as-received material and the material processed at pressures of 2 GPa and 4 GPa were single phase but the material processed at 8 GPa contained...