Glass phase expelling during liquid phase sintering of YSZ

Expelling of the liquid phase during sintering of ZrO2-6.5 mol% Y2O3- 0.5 mol% Pr2O3 ceramic was observed as a result of grain coarsening. ZrO2- 7.0 mol% Y2O3 samples, without Pr2O3 addition, do not show this effect under the same sintering conditions. The expelling process is caused by surface tens...