Novel process for the production of 3Y-TZP ceramics: comparison between ageing in artificial saliva and accelerated ageing

The degradation of tetragonal zirconia polycrystalline (3Y-TZP) ceramics prepared by a novel film growth technique, and by sintering at 1400 °C, was evaluated for one year using two processes: (i) degradation under oral conditions in artificial saliva (37 °C and pH 6.8) and (ii) accelerated degradat...

Full description

Bibliographic Details
Main Authors: M C Aragón-Duarte, M Bocanegra Bernal, A Reyes-Rojas, H E Esparza-Ponce
Format: Article
Language:English
Published: IOP Publishing 2020-01-01
Series:Materials Research Express