Corrosion Behavior in Hydrochloric Acid of Pure Titanium after Ultrasonic Severe Surface Rolling
Designing a gradient nanostructure is regarded as an effective strategy for strengthening commercial pure Ti without seriously sacrificing ductility. However, the corrosion behavior of the gradient nanostructured (GNS) pure Ti is far from clear, especially in reducing acid in which pure Ti shows poo...