Recovery of Silver and Lead from Jarosite Residues by Roasting and Reducing Pyrometallurgical Processes
This work focuses on the recovery of lead and silver from jarosite waste by a three-stage process: drying, roasting and reduction at 100 °C, 700 °C and 1400 °C, respectively. A flux mixture with 48 mass% CaO and 52% SiO<sub>2</sub> was used for the reduction stage. A gas consisting of 70...