Effect of B4C reinforcement ratio and sintering temperature on the mechanical behavior in Al-B4C composites

In this study, powders of Al 1070 and B4C were prepared by volume in three different reinforcement ratios 4 % B4C, 8 % B4C and 16 % B4C compacted under the pressure of 500 MPa with cold pressing method then sintered under the temperatures of 500, 550 and 600°C. Then the hardness was measure...