Preparation of SiO2-diamond composites by spark plasma sintering

SiO2-diamond composites with 65–85 mass% diamond were fabricated by spark plasma sintering at 1873 K under 130 MPa for 300 s using bimodal diamond particle size of 2 and 25 µm in diameter. The diamond particles were coated with a SiC layer by chemical vapor deposition. The effects of diamond content...

Full description

Bibliographic Details
Main Authors: Mettaya Kitiwan, Hirokazu Katsui, Takashi Goto
Format: Article
Language:English
Published: Taylor & Francis Group 2021-07-01
Series:Journal of Asian Ceramic Societies
Subjects:
Online Access:http://dx.doi.org/10.1080/21870764.2021.1952745