Effect of extrusion ratio on microstructure and mechanical properties of Mg-6Sn-3Al-1Zn alloy

The Mg–6Sn–3Al–1Zn (wt%) alloy was prepared by casting and then deformed by hot extrusion at 350 °C with different extrusion ratios (9:1, 13:1, 20:1), extrusion rate was 20 mm min ^−1 . The microstructure of as-extruded alloy was analyzed by XRD and EBSD, the tensile properties were tested by a univ...

Full description

Bibliographic Details
Main Authors: Shihao Zhou, Fuan Wei, Jinhui Wang, Peipeng Jin
Format: Article
Language:English
Published: IOP Publishing 2022-01-01
Series:Materials Research Express
Subjects: