Changes in the structure and D desorptive release from W-D co-deposit layers caused by thermal annealing

The annealing of ∼1 μm thick tungsten–deuterium co-deposit layers produced at 320 ± 25 K is found to induce changes in the desorptive release behavior and crystal structure. The changes in co-deposits were revealed by annealing in the temperature range 273–1273 K, examining the crystal structure wit...