Reactions at the molten flux-weld pool interface in submerged arc welding
In submerged arc welding (SAW) of chromium (Cr) containing steels, Cr is usually added to the weld metal from the weld wire, and not from the welding flux. Manufacturing of weld wires of specific compositions is expensive and time consuming and cannot closely match all the desired alloy compositions...