Durability evaluation of surface softened steel bar for prestressed concrete

The effects of Si addition and surface softening on delayed fracture susceptibility were evaluated in tempered martensitic steels with tensile strength of 1450 MPa. The delayed fracture susceptibility was reduced when Si content was increased from 0.2 mass% to 1.88 mass%. The delayed fracture suscep...